Super Soft Smooth Hydrophilic Silicone Oil RH-NB-8098-9

Introduction

Super soft smooth hydrophilic silicone oil RH-NB-8098-9 is modified quaternary ammonium multi-copolymerized polymer polysiloxane.

 

Advantage

1. Endow fabric super soft and smooth hand feeling.

2.Can endow cotton fabric thick feeling.

3. No yellowing change, less discolour, no effect to color light.

4.Good hydrophilicity

5.Good stability, easy to repair

 

Basic Character

Appearance: little yellow transparentliquid

Ionicity: weak cationic

Solid content: 85-87%

 

Application

Apply to the soft hydrophilic finishing of woven and knitted cotton fabric.

 

Usage Amount for Reference 

Recommend to dilute 20% emulsion to use.

(1) Dipping Process:   RH-NB-8098-9 diluted emulsion   2-6%(o.w.f)

(2) Padding Process:   RH-NB-8098-9 diluted emulsion   10-40g/L

 

Package

 100kg or 190kg plastic barrel.

 

Storage

 Store in cool and ventilated warehouse. 6 months of storage period.

 

 

Emulsification Method

 

RH-NB-8098-9:           200kg

Emulsifier:                 40kg

Acid water:         5kg Glacial acetic acid+5kg water

Water:                     360kg

 

Dilute process:

1. Add RH-NB-8098-9 and emulsifier to reactor, start stirring for 5-10 minutes;

2. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;

3. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;

4. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;

5. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;

6. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;

7. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;

8. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;

9. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;

10. Slowly add rest water while stirring, add rest acid water, stir evenly for 5-10 minutes, add glacial acetic acid to adjust PH value to 5-6

 

Notice: Must use high speed machine, last time can add water slowly.

Emulsifier: XL40:XL90=1:1

When in cold weather, emulsifier is easily to freeze, heat and stir to thaw before use.